CRYSTAL STRUCTURE AND HIRSHFELD SURFACE ANALYSIS OF 4AZIDO-2-(4-METHOXYPHENYL)-5-(2-NITROPHENYL)-2H-1,2,3-TRIAZOLE SYNTHESIZED ON THE BASIS OF DIBROMODIAZADIENE


Abdullayeva A. A., Ahmedova N. E., Atakishiyeva G. T., Ahmedova I. C., Babazade B. M., Akkurt M., ...Daha Fazla

NEW MATERIALS COMPOUNDS AND APPLICATIONS, cilt.8, sa.2, ss.149-161, 2024 (ESCI, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 8 Sayı: 2
  • Basım Tarihi: 2024
  • Doi Numarası: 10.62476/nmca82149
  • Dergi Adı: NEW MATERIALS COMPOUNDS AND APPLICATIONS
  • Derginin Tarandığı İndeksler: Emerging Sources Citation Index (ESCI), Scopus
  • Sayfa Sayıları: ss.149-161
  • Anahtar Kelimeler: Triazole, hirsfield surface analyse, noncovalent interactions
  • Erciyes Üniversitesi Adresli: Evet

Özet

The newly synthesized title compound was subjected to characterization via NMR and single crystal X-ray diffraction techniques. A Hirshfeld surface analysis was performed to analyze intermolecular interactions. Stabilization of molecular packing is achieved by a strong C---H...O hydrogen bond, C---H...it it and it-it it interactions.